Chemistry: Cathode
Pages 203–232 (30 pages)
Text on page 207
Impact Of Nickel Content On The Performance And Applications Of NCM And NCA Cathodes NCM 5-series*
NCM 6-series
NCM8-series
NCM 9-series
Polycrystal
Single Crystal
Polycrystal
Single Crystal
Polycrystal
Single Crystal
Polycrystal
Single Crystal
Capacity (mAh/g)
Price USD/mt 01/02/25
11,386 (consumables)
13,588 NEV, new energy vehicles)
13,119 (consumables)
14,489 NEV
15,237 (consumables) 16,980 NEV
NCA 8-series
High-Ni materials must be annealed in O2, whereas mid-Ni materials can be annealed in air. High-Ni materials require LiOH as the lithium source, while mid-Ni materials can use Li2CO3; LiOH may lead to equipment corrosion. High-Ni materials are more sensitive to humidity compared to mid-Ni materials, resulting in higher lithium residuals.
Process difficulty
Advantage
Good performance balance and relatively low cost
Moderate energy density, good cycle life, and safety
High energy density, high stability
High energy density and therefore lower cost per kWh
Good energy density, good rate capability, better stability
Applications
EV
EV
EV
Heavy duty EV Long range EV
EV, Powertools, twowheelers.
5-series means there are 50% Ni in the composition Source: MTI, MSE, Fangzheng Report, SMM