Cell Design and Materials: Li-Ion
Pages 297–359 (63 pages)
Text on page 306
NMC 523 vs 622 vs 811 Mid-Ni NMC variants NMC622 / NMC523
Offer the best overall balance between performance materials/manufacturing costs and stability Good for Mid-class/Entry EVs and BESS
High-Ni NMC811:
Maximize energy density, however stability and degradation issues require special engineering (doping/coating, electrolyte additives and BMS control) to be viable Valuable for high range/performance applications (e.g, Premium Class of Long-range EVs)
Parameter
NMC523
NMC622
NMC811
Relative Energy Density
Baseline
Higher (ca. 510% vs 523
Highest (best Wh/kg)
Thermal Stability
Best
Middle
Lowest
Cycle Life
Good
Balanced
Shorter
Charging/SOC
Faster charge, tolerant to higher Balanced SoC
High SoC accelerate degradation
Material Cost
Higher 30% Co
Lower than 523 20% Co
Lowest 10% Co
Manufacture Complexity
Easiest
Moderate
Hardest
Technology Approach
Particle morphology, coating, electrolyte additives
Doping/coating, reshaping
Doping/coating, gradient particles, electrolyte additives, BMS control
Application(s) Targeted
Entry class EVs; energy storage
Mainstream EVs
Premium high performance EVs with high range
Manufacturing complexity (advance engineering, moisture control, high yield losses and quality control requirements) limits high–Ni penetration In the China historically mid-Ni NMC chemistries are dominant (especially NMC622, whereas NMC811 is present in niche premium/export EV segment In the Europe and North America NMC811 is growing the share in EV due to the focus on higher energy density Source: 1 Y. Ding et al. Electrochem. Energy Rev., 2019, 2, 128.; 2 M. S. E. Houache et al. Batteries, 2022, 8, 70.; 3 T&E Report 2023 Clean and lean: Battery metals demand from electrifying cars, buses and coaches.; 4] https://www.adamasintel.com/mid-nickel-ev-batteries-garner-19-market-share-in-china/
Extracted from the PDF; charts and images may read imperfectly.