Cell Design and Materials: Li-Ion
Pages 297–359 (63 pages)
Text on page 342
Silicon Basic Technology and Information Engineered silicon increases anode specific capacity as a blend with or replacement for graphite in Li-ion batteries LIBs Silicon alloys with lithium (fully lithiated silicon Li15Si4 to deliver a theoretical specific capacity of ~3,572 mAh/g, approximately an order of magnitude higher than graphite, making it highly attractive for cell energy density. However, silicon undergoes ~300400% volume expansion during lithiation, leading to mechanical fracture, unstable SEI formation, and rapid capacity fade. Consequently, silicon anodes are implemented through engineered architectures and low-percentage blending strategies to balance energy density gains with cycle life and manufacturability required for EV applications.
SILICON MONOXIDE SiOx
SILICON IN CARBON Si-C
Metallic SILICON Si
Production process: SiOx is produced via high-temperature vapor-phase synthesis followed by condensation and milling to form silicon-oxygen composite powders with controlled oxygen content. oxidation buffers volume expansion and stabilized SEI formation, enabling improved cycle life + Partial and manufacturability compared to elemental silicon. – Lower active silicon fraction limits achievable capacity gain, typically restricting SiOx usage to low blending ratios 10%) in anodes.
PROPERTIESPERFORMANCE LINKAGE Silicon anode performance is governed by particle size, oxygen content, carbon architecture, and interfacial stability, which collectively determine achievable capacity, cycle life, and fast-charging robustness.
Production process: Si-C composites are produced by embedding nano- or micro-scale silicon within engineered carbon matrices via CVD, or pyrolysis.
Carbon matrices provide electrical conductivity and mechanical confinement to restrain volume expansion, improving cycling stability and rate capability while enabling higher silicon loadings than SiOx.
EV DRIVEN SILICON ANODE STRATEGIES
Carbon dilution and complex processing reduce gravimetric energy density benefits and increase manufacturing cost.
Near-term EV adoption: Low-percentage silicon blending (primarily SiOx for incremental energy density gains.
Mid-term pathways: Engineered Si-C composites to balance capacity and durability.
Long-term potential: Higher silicon loadings enabled by structural and interfacial innovations.
Production process: Metallic silicon anodes are produced via metallurgical grinding for micro-silicon or CVD-based deposition of nano-silicon on graphite or current collectors.
High silicon content enables the largest potential increase in anode specific capacity. Severe volume expansion and unstable interfacial behavior lead to rapid degradation, limiting direct EV deployment without advanced structural or interfacial mitigation.
Source: Mazir Ashuri et al 2023 Silicon oxides for Li-ion battery anode... Journal of Power Sources, 559. Iwamura, S. et al 2015 Li-Rich Li-Si Alloy as a Lithium-Containing... Sci Rep, 5, 8085. Zhang et al 2023 Recent advances of SiOx-based anodes... Nano Research Energy, 23. Zuo, Xiuxia et al 2017 Silicon based lithium-ion battery anodes... Nano Energy, 311, 113143. P.U. Nzereogu et al 2022 Anode materials for lithium-ion batteries... Applied Surface Science Advances, 9.. Battery Report 2023, Battery Report 2024
Extracted from the PDF; charts and images may read imperfectly.
Page 342 · 46/63